PEI 基礎(chǔ)創(chuàng)新 (美國) 2100
原料技術(shù)數(shù)據(jù)
性能項目 |
試驗條件[狀態(tài)] |
測試方法 |
測試數(shù)據(jù) |
數(shù)據(jù)單位 |
基本性能 |
吸水率 |
24小時,73?H |
ASTM D-570 |
0.210 |
% |
吸水率 |
平衡,73?H |
ASTM D-570 |
1.20 |
% |
熔體流動速率 |
--- |
ASTM D-1238 |
6.3 |
g/10min |
物理性能 |
模具收縮率 |
--- |
ASTM D-955 |
5-6 |
in/inE-3 |
固體比重 |
--- |
ASTM D-792 |
1.34 |
--- |
機械性能 |
屈服抗拉強度 |
--- |
ASTM D-638 |
16600 |
Psi |
屈服抗拉伸長 |
--- |
ASTM D-638 |
5.0 |
% |
斷裂抗拉伸伸長 |
--- |
ASTM D-638 |
6.0 |
% |
屈服撓曲強度 |
--- |
ASTM D-790 |
29000 |
Psi |
撓曲模量 |
--- |
ASTM D-790 |
650000 |
Psi |
洛氏硬度 |
--- |
ASTM D-785 |
114 |
Psi |
IZOD無缺口沖擊強度 |
--- |
ASTM D-4812 |
9.0 |
ft-lb/in |
IZOD缺口沖擊強度 |
--- |
ASTM D-256 |
1.1 |
ft-lb/in |
電氣性能 |
體積電阻率 |
--- |
ASTM D-257 |
1×1017 |
Ω.cm |
介電強度 |
62mils |
ASTM D-149 |
700 |
V/mil |
介電常數(shù) |
1KHz |
ASTM D-150 |
3.50 |
--- |
損耗因數(shù) |
1KHz |
ASTM D-150 |
0.0014 |
--- |
熱 性 能 |
燃燒性 |
--- |
UL 94 |
V-0 |
class |
熱指數(shù) |
電性能 |
機械沖擊性能 |
非機械性能 |
|
--- |
|
|
|
維卡軟化點 |
--- |
ASTM D-1525 |
434 |
?H |
熱變形溫度 |
66Psi |
ASTM D-648 |
410 |
?H |
熱變形溫度 |
264Psi |
ASTM D-648 |
405 |
?H |
|
--- |
|
|
|