耐寒PC EXL1414T 沙伯基礎(chǔ)SABIC LEXAN PC EXL1414T
LEXAN? EXL1414T resin
聚碳酸酯PC
SABIC Innovative Plastics Asia Pacific
PC EXL1414T 產(chǎn)品說明:
LEXAN EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL1414T resin is a general purpose product available in transparent and opaque colors and is an excellent candidate for a broad range of applications.
物理性能
|
額定值 |
單位制 |
測試方法 |
比重 |
1.19 |
g/cm3 |
ASTM D792, ISO 1183 |
熔流率(熔體流動速率) (300°C/1.2 kg) |
10 |
g/10 min |
ASTM D1238 |
溶化體積流率(MVR) (300°C/1.2 kg) |
9.50 |
cm3/10min |
ISO 1133 |
收縮率 |
|
|
內(nèi)部方法 |
流動 : 3.20 mm |
0.40 到 0.80 |
% |
|
橫向流動 : 3.20 mm |
0.40 到 0.80 |
% |
|
吸水率 |
|
|
ISO 62 |
飽和, 23°C |
0.12 |
% |
|
平衡, 23°C, 50% RH |
0.093 |
% |
|
硬度 |
額定值 |
單位制 |
測試方法 |
洛氏硬度 (L 計秤) |
87 |
|
ISO 2039-2 |
機(jī)械性能 |
額定值 |
單位制 |
測試方法 |
拉伸模量 |
|
|
|
-- 3 |
2190 |
MPa |
ASTM D638 |
-- |
2310 |
MPa |
ISO 527-2/1 |
抗張強(qiáng)度 |
|
|
|
屈服 4 |
57.6 |
MPa |
ASTM D638 |
屈服 |
56.8 |
MPa |
ISO 527-2/50 |
斷裂 4 |
59.1 |
MPa |
ASTM D638 |
斷裂 |
55.3 |
MPa |
ISO 527-2/50 |
伸長率 |
|
|
|
屈服 4 |
5.6 |
% |
ASTM D638 |
屈服 |
5.4 |
% |
ISO 527-2/50 |
斷裂 4 |
120 |
% |
ASTM D638 |
斷裂 |
110 |
% |
ISO 527-2/50 |
彎曲模量 |
|
|
|
50.0 mm 跨距 5 |
2180 |
MPa |
ASTM D790 |
-- 6 |
2120 |
MPa |
ISO 178 |
彎曲應(yīng)力 |
|
|
|
-- 6, 7 |
88.6 |
MPa |
ISO 178 |
屈服, 50.0 mm 跨距 5 |
92.0 |
MPa |
ASTM D790 |
沖擊性能 |
額定值 |
單位制 |
測試方法 |
簡支梁缺口沖擊強(qiáng)度 8 |
|
|
ISO 179/1eA |
-30°C |
60 |
kJ/m2 |
|
23°C |
70 |
kJ/m2 |
|
簡支梁無缺口沖擊強(qiáng)度 8 |
|
|
ISO 179/1eU |
-30°C |
無斷裂 |
|
|
23°C |
無斷裂 |
|
|
懸壁梁缺口沖擊強(qiáng)度 |
|
|
|
-30°C |
710 |
J/m |
ASTM D256 |
23°C |
820 |
J/m |
ASTM D256 |
-30°C 9 |
55 |
kJ/m2 |
ISO 180/1A |
23°C 9 |
65 |
kJ/m2 |
ISO 180/1A |
無缺口伊佐德沖擊強(qiáng)度 9 |
|
|
ISO 180/1U |
-30°C |
無斷裂 |
|
|
23°C |
無斷裂 |
|
|
裝有測量儀表的落鏢沖擊 |
|
|
ASTM D3763 |
-30°C, Total Energy |
77.4 |
J |
|
23°C, Total Energy |
75.5 |
J |
|
熱性能 |
額定值 |
單位制 |
測試方法 |
載荷下熱變形溫度 |
|
|
|
1.8 MPa, 未退火, 3.20 mm |
121 |
°C |
ASTM D648 |
1.8 MPa, 未退火, 64.0 mm 跨距 10 |
116 |
°C |
ISO 75-2/Af |
維卡軟化溫度 |
|
|
|
-- |
139 |
°C |
ASTM D1525 11, ISO 306/B120 11 |
-- |
138 |
°C |
ISO 306/B50 |
Ball Pressure Test (125°C) |
通過 |
|
IEC 60695-10-2 |
線形熱膨脹系數(shù) |
|
|
|
流動 : -40 到 95°C |
6.7E-5 |
cm/cm/°C |
ASTM E831 |
流動 : 23 到 80°C |
6.7E-5 |
cm/cm/°C |
ISO 11359-2 |
橫向 : -40 到 95°C |
8.0E-5 |
cm/cm/°C |
ASTM E831 |
橫向 : 23 到 80°C |
8.0E-5 |
cm/cm/°C |
ISO 11359-2 |
RTI Elec |
130 |
°C |
UL 746 |
RTI |
130 |
°C |
UL 746 |
電氣性能 |
額定值 |
單位制 |
測試方法 |
表面電阻率 |
> 1.0E+15 |
ohms |
ASTM D257 |
體積電阻率 |
> 1.0E+15 |
ohms·cm |
ASTM D257 |
可燃性 |
額定值 |
單位制 |
測試方法 |
UL 阻燃等級 |
|
|
UL 94 |
0.8 mm |
HB |
|
|
3.0 mm |
V-2 |
|
|
灼熱絲易燃指數(shù) (3.0 mm) |
960 |
°C |
IEC 60695-2-12 |
熱燈絲點火溫度 |
|
|
IEC 60695-2-13 |
0.8 mm |
850 |
°C |
|
3.0 mm |
850 |
°C |
|
光學(xué)性能 |
額定值 |
單位制 |
測試方法 |
透射率 (2540 μm) |
82.0 |
% |
ASTM D1003 |
霧度 (2540 μm) |
3.0 |
% |
ASTM D1003 |
注射 |
額定值 |
單位制 |
|
干燥溫度 |
121 |
°C |
|
干燥時間 |
3.0 到 4.0 |
hr |
|
干燥時間,最大 |
48 |
hr |
|
建議的最大水分含量 |
0.020 |
% |
|
建議注射量 |
40 到 60 |
% |
|
料筒后部溫度 |
271 到 293 |
°C |
|
料筒中部溫度 |
282 到 304 |
°C |
|
料筒前部溫度 |
293 到 316 |
°C |
|
射嘴溫度 |
288 到 310 |
°C |
|
加工(熔體)溫度 |
293 到 316 |
°C |
|
模具溫度 |
71.1 到 93.3 |
°C |
|
背壓 |
0.345 到 0.689 |
MPa |
|
螺桿轉(zhuǎn)速 |
40 到 70 |
rpm |
|
排氣孔深度 |
0.025 到 0.076 |
mm |
|
耐寒PC EXL1414T 沙伯基礎(chǔ)SABIC LEXAN PC EXL1414T。以上是耐寒PC EXL1414T物性數(shù)據(jù)。如需了解耐寒PC EXL1414T單價、交期或其它塑膠原料信息、請聯(lián)系我們!